SERA will not help you - it is only a tool to measure tin /copper
concentrations . We have been running immersion tin for 5 years with no
issues but only one thermal excursion is allowed. The tin forms a
copper/tin intermetallic after thermal. We even silkscreen before tin to
eliminate this bake cycle. Regards Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Wednesday, June 19, 2002 12:07 PM
To: [log in to unmask]
Subject: Re: [TN] Immersion Tin
Hi Tony,
we experienced poor wave soldering after 2 reflows with immersion tin.
So,
please give me a few hints on SERA. Is it a test that the board house
will
do, or it has to be at our incoming? Does it imply additional charges?
Where
can I read more?
Thanks,
Ioan
> -----Original Message-----
> From: tony steinke [SMTP:[log in to unmask]]
> Sent: Wednesday, June 19, 2002 11:19 AM
> To: [log in to unmask]
> Subject: Re: [TN] Immersion Tin
>
> Grant,
> Having installed the Cookson(Dexter) FST chemistry a couple of years
> ago at my previous employer, there are concerns that you should be
aware
> of.
> The immersion tin
> process is a beautiful thing if applied and processed properly. Some
of
> the
> major
> issues that I experienced were:
> Solder mask adhesion(you should tape test any incoming product)
> Request that SERA(sequential electromigration reduction analysis) test
be
> performed.
> And the biggest problem was getting acceptable solderability on second
> pass
> wave solder
> or second pass solder paste. The copper migration greatly accelerates
> during
> any thermal
> excursion, but that is what the SERA testing will show you.
> Tony Steinke
> [log in to unmask]
>
> ----- Original Message -----
> From: "Grant Emandien" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Wednesday, June 19, 2002 3:06 AM
> Subject: [TN] Immersion Tin
>
>
> > Members,
> >
> > A PCB supplier has requested us to evaluate immersion tin as a
finish.
> > Immediate concerns raised were shelf life, solderability, whiskers,
etc.
> > Researching the archives has noted similar as well as opposing views
and
> > concerns. In addition to possible problems arising from immersion
tin
> > finish, what PCB fabricator process changes may contribute to
possible
> > reliability and solderability concerns and how this impacts
production
> > processes such as reflow. The proprietary chemistry used is MacStan
HSR
> from
> > Macdermid.
> >
> > Anyone willing to share experiences and guide me towards making an
> informed
> > decision.
> >
> > TIA
> > Grant
> >
> >
> >
**********************************************************************
> > Notice:
> >
> > This email transmission contains confidential information which is
the
> property of the sender. The information is intended only for the use
of
> the
> addressee. If you are not the intended recipient, you are hereby
notified
> that any disclosure, copying or distribution of the contents of this
> e-mail
> transmission, or the taking of any action in reliance thereon or
pursuant
> thereto, is strictly prohibited. Should you have received this email
in
> error, please immediately notify us by telephone to arrange for return
of
> the documentation comprising this transmission. In no event will
Tellumat
> (Pty) Ltd or the sender of this email be liable to any party for any
> direct,
> indirect, special or other consequential damages for any use of this
> email,
> or on any other hyper linked website, including, without limitation,
any
> lost profits, business interruption, loss of programs or other data on
> your
> information handling system or otherwise, even if we are expressly
advised
> of the possibility of!
> > such damages.
> >
> >
**********************************************************************
> >
> >
>
------------------------------------------------------------------------
--
> -------
> > Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> > To unsubscribe, send a message to [log in to unmask] with following
text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send e-mail to
[log in to unmask]:
> SET Technet NOMAIL
> > To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> > information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
> ext.5315
> >
>
------------------------------------------------------------------------
--
> -------
>
>
------------------------------------------------------------------------
--
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
[log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
> ext.5315
>
------------------------------------------------------------------------
--
> -------
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|