Hi Mike,
That was a great reply by Phil, and I will certainly be using what Phil has
said to strengthen my case as I too am going through exactly the same
scenario as you Mike.
I have recently written a report (using JEDEC-033) outlining the main issues
with MSD, the consequences and actions that need to be taken. The report has
a particular emphasis on BGA's as we can "actually prove" that moisture
ingress through bad storage practice effects this particular component. As
you have mentioned, with conventional components, MSD has been a very grey
area as it is quite hard to prove if or how it effects components, so I am
coming in on the BGA angle in the hope of putting in place a procedure for
all MSD components.
Please email me privately if you want any more info, or how I set out my
report.
Regards,
Adrian Hanks.
Production Engineer
atl telecom
············
========================
Cypress Drive
St Mellons
Cardiff CF3 OEG
Tel: +44 (029) 2050 0700
Fax: +44 (029) 2050 0701
E-mail: [log in to unmask]
Web: http://www.atlTelecom.com/
-----Original Message-----
From: Mike Hughes [mailto:[log in to unmask]]
Sent: 13 June 2002 01:04
To: [log in to unmask]
Subject: [TN] Moisture Sensitive Devices
I am the Purchasing Manager for a medium size Australian R&D company
involved in design and manufacture of radar & comms products for military
and civil government use.
We use almost 100% smd on our PCA's.
I have been alerted to the MSD issue and have read as much as I can get my
hands on from the IPC/JEDEC J-STD-033 and other articles to various other
publications.
It reads as a very serious issue that could be very costly to deal with.
I am putting together a paper to present to senior management on the issue,
its consequences and how my company should deal with it.
My problem is that whenever I speak to others in the industry I am told that
the whole issue is little more than a beat-up and I should ignore it and it
will go away.
Can anyone out there come back to me and give me the benefit of your
experiences and how you solved the issue.
Mike Hughes
Purchasing Manager
CEA Technologies Pty Ltd
Ph:02 6213 0050
Fx:02 6213 0053
www.cea.com.au
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------
Disclaimer of Liability
Ascom shall not be held liable for any improper or incorrect use of
the information described and/or contained herein and assumes no
responsibility for anyone's use of the information. In no event shall
Ascom be liable for any direct, indirect, incidental, special,
exemplary, or consequential damages (including, but not limited to,
procurement or substitute goods or services; loss of use, data, or
profits; or business interruption) however caused and on any theory
of liability, whether in contract, strict liability, or tort
(including negligence or otherwise) arising in any way out of the use
of this system, even if advised of the possibility of such damage.
---------------------------------------------------------------------
________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|