We use selective solder fixtures for situations like this. A little money up
front, but cheaper than rework. Check EMC Global at
http://www.emcgti.com/core/products/fixture_wsp.shtml . There are other
vendors, but I have only dealt with EMC so far.
=========================
Bob Barr
Manufacturing Engineering
Formation, Inc.
Voice: 856-234-5020 x3035
Fax: 856-234-6679
=========================
-----Original Message-----
From: Henry Rekers [mailto:[log in to unmask]]
Sent: Wednesday, June 26, 2002 10:08 AM
To: [log in to unmask]
Subject: [TN] Reflow on Wave.
Does anybody have any suggestions on avoiding reflow of a 357 ball bga on
the wave? I'm dealing with a 6 layer board and I've kept the preheat as low
as possible. Kapton tape doesn't seem to help. Has anybody tried any
custom manufactured sheilding?
Thanks.
Henry J. Rekers
Manufacturing Engineer.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|