A supported hole would be one, such as a via, where the barrel is
"supported" on either side of the board by a pad.
An unsupported hole would be one in which there is a pad on one side only,
and that pad is generally larger than if it were a supported hole.
Unsupported holes are used primarily on through hole devices.
Hope this helps
-----Original Message-----
From: Peter Lee [mailto:[log in to unmask]]
Sent: Tuesday, June 25, 2002 3:22 PM
To: [log in to unmask]
Subject: [TN] Definition of Suported/ unsupported hole
Technet,
Can anyone explain the difference between a supported
and unsupported hole on PCB?
I am reading a section on IPC-A-600 RevF and section
2.10.3/4 specify difference acceptance criteria
according to the hole type.
Rgds,
Peter
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|