offline? Hm..guess many more are interested. Had many words with Werner when we had a serious SBGA soldering problem. As I remember, weak solder joints were not found in the very IMC chain itself, but rather in a 'sick' interface layer close to the IMCs. XILINX helped us with the final investigation..and many others in this forum. The mentioned weak member was extremly thin <micron and hard to determinate. But that is history, and not a general case.
Regards
Ingemar Hernefjord
Ericsson Microwave Systems
PS. DELL our favorite, have hundreds of them. Never heard about solder problem in a DELL. Perhaps you screen out some bad? Joking, Victor..
-----Original Message-----
From: Victor Hernandez [mailto:[log in to unmask]]
Sent: den 19 juni 2002 15:46
To: [log in to unmask]
Subject: Re: [TN] Intermetallic Joint Failure
Henry/Werner,
I work in a Component/Material Analytical Lab. I conduct cross section
of all interconnection. I have found interconnection failures in BGA, the
failure will be: Fracture in the bulb solder, IMC region or nickel plating.
The problem with subsequence rework is did the PWB reach a reflow temp.
environment which can re-grow the IMC region. potential for a weak joint.
We can take this off line if so desired.
victor,
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Wednesday, June 19, 2002 7:48 AM
To: [log in to unmask]
Subject: Re: [TN] Intermetallic Joint Failure
Hi Henry,
The problem with "rework" is not IMC layers getting too thick, but the
damage
done to the solder joints of neighboring components and the PWB. In all my
years in reliability, I have never seen an "Intermetallic Joint Failure."
Best regards,
Werner Engelmaier
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|