Dear all
hello
We are facing a problem that the leads of components getting
tarnished(oxidized) in store only those which are the silver plated like BNC
connectors , bridge rectifiers, LED's etc. all are through hole type. The
humidity Laval varies 43 to 47 % .Is this is sufficient, Pls. suggest the
special storage for these components .Is this problem comes by defaults ?
and any method about the oxidized once re - using ?. Thanks in advance for
your any response.
With regards
Pankaj Karnwal
Quality Assurance
BESL NOIDA
PH .91-120-4420394-5 EXTN.211
e mail : <mailto:[log in to unmask]>
Barco, innovators in image processing
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|