I'm still here, still dealing with the new (used) Ominflo-10 issues that I
spoke of earlier.
I've found out that even though the oven has what's called a "Nitro-cool"
option, I don't need nitrogen per-se...I can use compressed air, since
ambient air is 80% nitrogen anyway.
There is the disclaimer in the manual that the machine may not operate
"normally" with a system designed for pure nitrogen using compressed air, but
doesn't get into the specifics of the abnormalities that may occur...can
anybody help with some real-world experiences?
I'd really love to connect with someone that uses these ovens, since this is
the first time that I've been exposed to the Omniflo-10...
I promise to not post non-techical emails, 'cept maybe on a rare occasion.
I'll put in the subject line "OT" at the beginning, so you can screen them
out...
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|