Bob
It should not be necessary if you apply sufficient on the under side,
IMHO. There is a risk that you may have somewhat more dangerous
residues, because this flux will never reach anything like soldering
temperature. If you want hi-rel, my guess would be to err on the safe
side, don't. If your app is low-cost consumer goods, used indoors, do
some qualification testing. In between, the choice is yours :-(
Brian
> Bob Arciolla wrote:
>
> We are using Kester 951 no-clean flux. Is it acceptable to either
> spray the component side of the printed circuit board and/or apply a
> drop of flux onto the component side hole to increase the amount of
> vertical fill and fix dewetting.
>
> Thanks Bob
>
> [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|