I have accomplished this with .010 X .0005 inch silver ribbon epoxied in
place along the board surface prior to reflow. Its tricky but can be done.
Do a good inspection at 10X mag minimum, prior to placing the device.
Good Luck,
Bruce Misner
> ----------
> From: Barbara Burcham[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Barbara Burcham
> Sent: Tuesday, June 11, 2002 5:12 PM
> To: [log in to unmask]
> Subject: [TN] Access to balls on a BGA from the opposite side of the
> Board
>
> We need to wire to two balls inside the perimeter of the BGA.
> Any one done this?
> Got ideas?
>
> Thanks,
> Barbara J. Burcham, CID
> PCB Designer
> [log in to unmask]
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|