Ken,
I searched sever years ago and had a hard time finding a document that wanted to nail down torques for a specific screw size. This is due to each application can have a different set of characteristics.
I did collect a bunch of material (SAE ARP 1928 was one of them) and we settled on the following as our " internal standards"
2-56 - 3 inlb
4-40 - 8 inlb
6-32 - 10 inlb
8-32 - 20 inlb
10-32 - 32 inlb
1/4-20 - 60 inlb
These values assume the screw is steel or stainless steel. For brass the values should be lower and for nylon the values should be even lower yet.
Keep in mind these are not hard and fast numbers. You should test your application for what works best.
Regards,
Phil Nutting
-----Original Message-----
From: Ken Carlile [mailto:[log in to unmask]]
Sent: Tuesday, June 11, 2002 10:06 AM
To: [log in to unmask]
Subject: [TN] IPC Torque Specifications
Does IPC have any Torque specifications for hardware mounting to FR-4? I
have searched the archives and only find peoples opinions. If IPC doesn't
have this does Mil Spec or ANSI?
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|