Mark,
In past lives I've seen polyimide labels used. These were printed in a thermal printer and the material would stay on through the wave solder. For an easy start, look in the Brady labeling catalog for examples. Another place to go is your "local" Identco rep.
http://www.bxcommerce.com/identco/contact_info.asp
Phil
-----Original Message-----
From: Mark Hargreaves [mailto:[log in to unmask]]
Sent: Wednesday, May 29, 2002 4:26 PM
To: [log in to unmask]
Subject: [TN] bare board serialization
Hi All,
I'm looking for a way to serialize bare boards & panel coupons to provide
traceability for IPC 6012 jobs. Can anyone suggest a tool & ink type?
Thanks,
Mark Hargreaves
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|