I presume you are talking about the glass reinforced version by Rogers and
Arlon's, lisenced from Rogers, CLTE. I last used in in a MLB design three
years ago with mixed results mostly because of "nearly" qualified fab
capabilities.
The boards were designed using the ceramic material combined with Getek. The
MLB's stayed together reasonably well but had some surface "flaking" issues
based on not being able to determine cure. The stuff would readily come off
when lightly sraped with a knife or other hard object.
Trident was the board shop in Carson City, NV and Ambitech, I belive, was
the other shop. Damn good R/F results though.
Earl Moon
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|