Dear Pete, I also made myself your question time ago, my relative truth is
that in all cases that you can use 2 plies used it, One ply means that the
ply system resin- reinforce must be in perfect state, no fault is admitted.
I never had meet an adhesion problem using one ply,
but i had meet dielectrical lacks betw. layer and was due to operational
asemblies fault.
at the end is as we say :is not the same the double than the half
regards,
lino
>From: Pete Jones <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>, Pete Jones
><[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] FAB Question: laminate - 1 ply or 2??
>Date: Thu, 25 Apr 2002 09:55:27 -0400
>
>Hello all TechNetters,
>
>What is the difference between using 1 ply of laminate or 2 in fab boards?
>
>Is there a REAL concern that 1 ply will not be sufficient electrical
>insolation? Or has resins now evolved enough to make it safe to use just
>one
>ply?
>
>I deal mostly, but not exclusively, with the military and would like to
>make
>sure of my statement that 1 ply should be sufficient. Can I get reliable
>references anywhere concerning this issue, one way or the other?
>
>Thanks to all participants in this discussion.
>
>Pete
>
>_________________________________________________________________
>Join the world’s largest e-mail service with MSN Hotmail.
>http://www.hotmail.com
>
>---------------------------------------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
>SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------------
_________________________________________________________________
Únase con MSN Hotmail al servicio de correo electrónico más grande del
mundo. http://www.hotmail.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|