Look at IPC-A-620, figure 5-45. If you want confidence, go to the
manufacturers spec for the contact and pull test a sample(s) (with the same
configuration) to be sure the tensile strength meets the manufacturers
recommendations, or alternately you can cross-section a sample to ensure the
strands are deformed and fill the voids.
---------------------------------------------------------------------------------