Silver finds it's way into high energy switchgear contacts (not solder
terminations) due to it's ability to maintain a functional contact surface
in the presence of arcing. Normal contamination of surfaces is defeated
through the wiping action forced on these contacts, when in transition.
Arcing and static surfaces of the contact are partitioned, where possible.
High rel components (mtbf still sucks) are hermetically sealed.
The mfring process is generally hostile to all switchgear; uncovered or
unsealed parts require special handling to reduce fallout.
Silver has no greater suitability for forming reliable solder joints, on or
in switchgear, than it has anywhere else.
A month is a very short time to guarantee solderability. Have you looked at
the date-codes on some of your electromechanical parts?
RL
[log in to unmask]
----- Original Message -----
From: "Jack C. Olson" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, April 17, 2002 8:38 AM
Subject: Re: [TN] Immersion Silver
> The PCD magazine list went down before I could get an
> answer to this question, does anyone have experience
> with silver and contact switches?
>
> ==============================================
>
> Most sources say a silver surface will not be solderable
> after a month or so unprotected. (Even in a baggie it will
> be okay a year later?)
> Anyway, you say it is good for switches, which would solve
> some of our hard gold plating problems.
>
> But I would think the "unsolderability" of the aged silver
> surface (unprotected in the unit and tarnished?) would
> affect the reliability of the switches, wouldn't it?
>
> Jack
>
>
>
>
>
>
> Rob Mongey <[log in to unmask]>@freelists.org
> 4Apr2002 06:08 AM
>
> Please respond to [log in to unmask]
>
> Sent by: [log in to unmask]
>
>
>
> To: [log in to unmask]
> cc:
>
> Subject: [pcdlist] Re: Immersion Silver
> Retain Until: 05/04/2002 Retention Category: G90 - Information and Reports
> Caterpillar Confidential: Green
>
>
>
> Hi all,
> Good to see Immersion Silver is starting to take off. We've been
using
> it
> in here for about two years, and it is now our prefered board finish (We
> get silver finish unless we specify differently.) More common useage will
> mean that maybe more Far Eastern shops will start supplying it.
>
> We started to use Silver because it is so adaptable to what we need
> our
> PCB surface finish to do, namely:
>
> 1. Good solderability. (Silver excels at this, ask any vendor).
> 2. Flatness for fine pitch SMT. (Silver is as flat, if not flatter than
> Gold)
> 3. Mechanical strength for carbon pill switch contacts / Elastomer
> contacts. ( Flash Gold is weak, and hard Gold gives SMT solderability
> problems)
> 4. Stability for compression power contacts. (We have power contacts on
our
> PCBs that mate to battery contacts via a spring compression. We found that
> the nickel under gold can cause problems with electrochemical migration
> toward our battery contact.)
>
> Immersion silver is the most suitable choice that can do all four. I'd use
> gold as an alternative, but we'd have to compromise our designs somewhat.
>
> We specify our Silver finish as 0.1 Microns Min to 0.2 Microns Max, over
> bare copper. Anyone else do it differently? Or do we trust our board
shops?
> :)
>
> Regards,
> Rob Mongey.
> CAD Technician.
>
> Robert Mongey <[log in to unmask]> Tel : +353 (0)91 774300
> Bio Medical Research Direct : +353 (0)91 774338
> BMR House, Fax : +353 (0)91 774302
> Parkmore Business Park West, Mobile : +353 (0)87 2485262
> Galway
> Rep of Ireland.
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|