Murata, at http://www.murata.com have a good article on this subject. Mainly
the reason is, that the aluminum electrolytic will loose 50% of the rated
capacitance a -40 degrees C. At -55C it is worse. This then also is true for
industrial applications. I just looked for the article that I am referring
to and couldn't find it, so I am attaching it.
Michael Wright
Sr. Engineer
ITT Cannon
952-974-5813
-----Original Message-----
From: DUTTON Phil [mailto:[log in to unmask]]
Sent: Tuesday, April 02, 2002 1:48 AM
To: [log in to unmask]
Subject: [TN] Aluminium Electrolytics
Hello Technetters,
Mil-STD-5400 para 4.3.8.2 says that aluminium electrolytic capacitors shall
not be used in airborne electronic equipment.
Can anyone please explain why this is so?
thanks,
Phil.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
************************************
If this email is not intended for you, or you are not responsible for the
delivery of this message to the addressee, please note that this message may
contain ITT Privileged/Proprietary Information. In such a case, you may not
copy or deliver this message to anyone. You should destroy this message and
kindly notify the sender by reply email. Information contained in this
message that does not relate to the business of ITT is neither endorsed by
nor attributable to ITT.
************************************
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|