Another late entry:
There's an old Bell System test for coatings. The outline is below.
1. Saturate a filter paper with an aqueous soln of 0.4M Na2CO3 and 0.1M
NaCl.
2. Sandwich the filter paper and a blotter sheet
between the test sample and a metal plate so the filter paper is in contact
with the test sample. Good contact with the test sample is essential!
3. Connect a dc power supply between the test sample (positive) and the
metal plate (negative) and set the current to 5ma/cm2 and maintain for
30s.
4. Remove the filter paper and develop in a 1% solution of Dimethylglyoxime
in a solvent made of 95%v/v EtOH and 5%conc NH4OH.
5. Count the developed red spots using 10X mag.
6. Typical pore counts for hard Au over Ni are:
>50 µinch: <20 pores/cm2
30µinch: <30pores/cm2
25µinch: <50pores/cm2
-----Original Message-----
From: Geoff Layhe [mailto:[log in to unmask]]
Sent: Tuesday, April 16, 2002 8:05 AM
To: [log in to unmask]
Subject: Re: [TN] Nickel Test
A late reply on this but I knew I had some information on porosity testing
hidden away somewhere.
Dimethylglyoxime is a spot test reagent for nickel in the presence of
ammonia. As far as I can remember the dmg was dissolved in iso-propyl
alcohol (approx 2%)and ammonia added. This solution turns red in the
presence of nickel, and was used as a porosity test for gold on nickel.
I don't have this method for porosity but I do have one using nioxime. This
test was used for porosity of electroplated gold on electroplated nickel on
copper. The minimum coating thicknesses were 2.5 microns (0.0001")gold on 5
microns (0.0002") nickel.
The test uses pressure and current so I doubt if it will be OK for the thin
enig coatings.
If you want the text of the test let me know your fax No.
Geoff Layhe
www.lamar-uk.co.uk
-----Original Message-----
From: Rudy Sedlak [mailto:[log in to unmask]]
Sent: 11 April 2002 02:25
To: [log in to unmask]
Subject: [TN] Nickel Test
I recall seeing a spot test for Nickel that involved using a solution of
Dimethylglyoxime in dilute Ammonia, + ???? as a spot test for gold porosity
to show presence of Nickel.
Does anyone have the exact details of this test? Does anyone know if it
works on Electroless Nickel? (Suspect it may not because EN is so much more
passive.)
Rudy Sedlak
RD Chemical Company
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
Private & Confidential:
This e-mail message is confidential and is intended solely for the person or
organisation to whom it is addressed. If the message is received by anyone
other than the addressee please return the message to the sender by replying
to it and then delete the message from your computer.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|