Hi MoonMan,
>OK, but I'm not able to directly correlate design guidelines
>with acceptance criteria in IPC requirement - not guidelines especially now
>that DoD has adopted and, essentially, validated the specifications - not
>guidelines.
IPC-610 ONLY assures SJ quality--that is not the same as reliability. While
quality of course is necessary for reliability, it is not sufficient--see
IPC-D-279.
So, now the Q is what is it you need to correlate. Also, I do not see the gap
you are referring to; please elucidate.
Werner Engelmaier
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|