Phil
I don't recommend any Al (or alloys) to Cu or Sn/Pb junction, where they
are in electrical contact. The electrochemical potential is sufficiently
great that corrosion is inevitable if they got damp, with all sorts of
nasties potentially migrating over the board surface. Al would be OK if
there were no electrical contact.
Brian
Phil Nutting wrote:
>
> Good afternoon TechNet,
>
> Would anyone like to share their knowledge about using an aluminum standoff as a conductor when connecting two circuit boards together. I suspect that if it were aluminum to copper there would be an issue, but what about aluminum to HASL surface of circuit boards?
>
> Thanks in advance for your wisdom,
>
> Phil Nutting
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|