I'd be willing to talk to one or two older codgers with J STD 001 and Mil
Spec experience to help my company move from one to the other. We're about 7
yrs. late - please suggest names or contacts - perhaps a one month contract
agreement. (consultant-type) - humble, please, not arrogant.
-----Original Message-----
From: Randy Bock Sr. [mailto:[log in to unmask]]
Sent: Friday, April 19, 2002 6:52 AM
To: [log in to unmask]
Subject: Re: [TN] OSP
This is the best reply yet.. THANK YOU
----- Original Message -----
From: Wenger, George M. <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, April 18, 2002 9:53 PM
Subject: Re: [TN] OSP
> Earl,
>
> I'd like to expand and comment on you question "Where have all the board
people gone, long time passing". Unfortunately the board people whet by the
wayside just like many other technical people. Companies have down sized
their technical efforts and increased their supply chain efforts with the
rational that we don't have to pay for technical information because our
suppliers will give us what we need for free. Well the one thing most
people learn during their life time is you get what you pay for. In the
past 18 months or more the attendance at technical conferences and seminars
has decreased, the technical content in email forms such as TechNet have
decreased and when you ask a supplier for technical date you get sales
information.
> I'm not sure how or if there is going to be a reversal but I sure hope
that young engineers entering the work place keep letting their management
know that engineering date not sales information is needed to make informed
decisions and effective risk assesments.
>
> -----Original Message-----
> From: Earl Moon [mailto:[log in to unmask]]
> Sent: Thursday, April 18, 2002 3:15 PM
> To: [log in to unmask]
> Subject: Re: [TN] OSP
>
>
> Outstanding Rick,
>
> I agree and side with Kerry as well but for his "boring" comment. I know
he
> meant well as we all try CPI.
>
> Other folks, me included, have commented on the lack of board type people
> participating enough on this forum. I certainly have done my best to get
> them back but probably have bored them and others to leaving because of my
> excessive time on the forum.
>
> Phil Hinton said this forum is becoming an "good old boys club" or some
such
> thing. I agreed then as now but we have the freedom to participate or not.
>
> I just want the facts man, just the facts. I have way more questions than
> answers but one thing is sure - we need more fabricators on this thing.
>
> I just finished a concurrent engineering conference with my assembler, my
> company, and my fab supplier. Excellent results concerning solder wetting,
> or not.
>
> Turns out our great fab supplier (Proto Engineering)provided highly
> solderable ENIG boards that didn't look that great after assembly in some
> areas. Also turns out, our fantastic assembler (MPI) uses the latest DEK
> stencil printers with ProFlo heads. Because of this, and the large pads
> required for a few parts, MPI requested steicils with "window pane"
> apertures for these large pads. Hence, non wetting on some pad areas. New
> one to me but greatly appreciated for us all.
>
> Where have all the board people gone, long time passing. I'll get of the
> fourm if it's me but we need fab folks no matter.
>
> MoonMan
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|