It is because of "usually nonimportant trivial things
that at times prove to be useful" that I am a reader of this forum!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Sauer, Steven T.
Sent: Friday, April 19, 2002 7:30 PM
To: [log in to unmask]
Subject: Re: [TN] Silver
To add to what Mel said: the reason for the disallowance had to do with the
susceptibility for "red plague" formation.
This is not to imply that I've been around longer than Mel, it was well
before my time but my mind is full of "usually nonimportant" trivial things
that at times prove to be useful!
Steve Sauer
Mfg Engineer
Northrop Grumman, Xetron
-----Original Message-----
From: Mel Parrish [mailto:[log in to unmask]]
Sent: Friday, April 19, 2002 10:16 AM
To: [log in to unmask]
Subject: Re: [TN] Silver
The content of 610 regarding silver plate wire is one of those dinosaurs
that is left over from the 70s and that originated in the very early Mil
Specs or maybe even NHB. You will not even find a reference in MIL-STD-2000
to restrict silver.
Contract documents and BOM commonly reference silver wire for production and
the justification as I recall was improved shelf life and solderability.
Additionally silver plate wire achieved preferred performance in
solderability testing after steam aging required under 202.
I'm sure there was a justification originally for the restriction but it was
before my time and that is saying sumpin.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|