Phil
What is your end application?
Leaving moisture in the board / assembly can lead to "milking or blooming",
a slight matt finish or milky appearance to the coating. This would be a bad
thing. Baking before coating, you could happily expose them to lower temps.,
provided that you increase the air movement over them as this will permit a
reduced drying time. e.g. 80 degC + >~ 2 M/sec air flow should work well,
maybe 10 to 15 minutes, but it will depend upon the geometry of the
assembly.
We have plenty of customers who clean and coat within 20 minutes or less,
without pre-baking - including automotive high-rel.
Regards Graham Naisbitt
[log in to unmask] <mailto:[log in to unmask]>
Concoat ANNOUNCE their acquisition of the former Multicore SPCID business.
MUST II Solderability Testing Systems -
CM Cleanliness Testing Systems -
Auto-SIR Reliability Testing Systems -
SoldaPro & NEW SoldaPro Wizard Thermal Profilers
For more information please visit our new web site: www.concoatsystems.com
<http://www.concoatsystems.com>
Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK
www.concoat.co.uk <http://www.concoat.co.uk>
Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Phil Nutting
> Sent: 08 April 2002 17:13
> To: [log in to unmask]
> Subject: [TN] Bake before Conformal Coat
>
>
> Good day, Technet
>
> After reviewing past threads regarding baking boards before
> conformal coating I come up with quite a varied selection of ideas.
> I found 1 hour @100°C, 4 hours at 150°C, and 4-5 hours at 125°C.
> My design engineer is concerned about the boards being exposed to
> this temperature for an extended time. Yes, in the wave solder it
> sees much higher temperatures... for a short period of time. Our
> aqueous wash system dries at about 65°C for 20 minutes.
> Our product normally is tested to 40 - 50°C depending on the
> customer needs.
> The past threads suggested raising the temperature above 100°C to
> "boil off" any remaining water.
>
> Can this time/temperature be narrowed down any?
>
> And if we use a lower temperature are we possibly trapping moisture?
>
> How will the reliability be affected by these elevated temperatures.
>
> Thanks in advance,
>
> Phil Nutting
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/scripts/wa.exe?S1=technet
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|