Hi Gary:
Its been a while since we talked.
The flux is applied to the SMT locations after the initial deposit is
flattened. Here is link to the flux being used.
http://www.midwestpcb.com/sales/Kehoe/Ecotack_SP37_SP37i.pdf
At the EASi Assembly Expo 1999 at McCormick Place then ran 3000 Sipad boards
through a fully automatic line.
Robert B. Denbo
MIS / Engineering Manager
Midwest Printed Circuit Services, Inc.
http://www.midwestpcb.com
mailto:[log in to unmask]
847.740.4120
847.740.4187 Fax
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Gary Camac
Sent: Monday, April 08, 2002 5:33 AM
To: [log in to unmask]
Subject: Re: [TN] Any SIPAD users?
Steve,
I would bet you can't feed these on a destacker. What's is the category of
flux being used? It is applied on the entire board surface or just at the
soldering locations?
Gary
Gary
----- Original Message -----
From: <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, April 05, 2002 6:33 PM
Subject: [TN] Any SIPAD users?
> Hi All!
>
> I got a few sample boards that a solid solder deposit was applied (SIPAD),
> along with what they call adhesive flux, to play around with. I got some
> dummy components and placed and reflowed them...I was very pleased with
the
> results!
>
> Do any of you use this technology? Any thoughts or opinions would be
> appreciated.
>
> Thanks!!
>
> -Steve Gregory-
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|