David,
I double checked the Tin thickness and you are right. 44 micron is too
thick. The correct measurement is .7 microns (~ 44 micro inches)
Thanks for catching that.
Tuan
"David Fish"
<[log in to unmask] To: "TechNet E-Mail Forum." <[log in to unmask]>, <[log in to unmask]>
> cc:
Subject: Re: Re: [TN] Immersion Gold Vs Immersion Tin for 0201 landpatterns
04/26/2002 06:18
PM
Imm tin at 44 micron!!! Wow, that seems very thick. We expect minimum
thickness of 0.65 microns with a maximum thickness of 1.5 microns.
Dave Fish
----- Original Message -----
From: "Tuan Bui" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, April 26, 2002 11:05 AM
Subject: Re: [TN] Immersion Gold Vs Immersion Tin for 0201 landpatterns
> Hi George,
>
> The Immersion Gold process that the PCB vendor stated that the Immersion
> gold (7-10 micron) over nickel over copper. The Immersion Tin process, as
> you have mentioned, is about 44 micron. It is good to hear that the
> immersion tin process can be easily/inexpensive reworked when its shelf
> live expires.
>
> BTW, thanks for your input.
>
> Tuan Bui
> Proc Dev Eng
> Conexant Systems Inc.
>
>
>
> George Milad
> <[log in to unmask]> To: [log in to unmask]
> Sent by: TechNet cc:
> <[log in to unmask]> Subject: Re: [TN]
Immersion Gold Vs Immersion Tin for 0201 landpatterns
>
>
> 04/26/2002 08:47
> AM
> Please respond to
> "TechNet E-Mail
> Forum."; Please
> respond to Gmilad
>
>
>
>
>
>
> Tuan,
> Could you clarify the "Immersion Gold" process that you are using. Is it
> Immersion gold over copper or it immersion gold over nickel over copper?
>
> Immersion Tin is a viable alternative for your application. However the
> thickness required will much higher than the 7 - 8 uins that you are
> presently using for gold, more like 30 - 40 uins. Tin is realtive
> inexpensive and can be easily reworked if shelf life becomes an issue.
>
> George Milad
> HDI Consulting
> Chairman IPC Plating Committee.
>
>
--------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
--------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|