Hi Peter,
At Plexus they have published a rather extensive report on the causes of
tombstoning. It included some remarks on the incidence of solder balls. Both
problem areas are partially caused by pad design on the board and aperture
design in stencils. (Some say the most significant factors for tombstoning
are pick-and-place accuracy and oven temperature profile.)
To minimize tombstoning the report indicates that pad design has a minimal
impact when using 0402-s, but for 0201-s you want to stay close to the
'normal' size for pad design.
To minimize solder balls it is recommended to change stencil apertures to
home plates. My personal preference (and that of some of our customers) is
to change the aperture to an oval, which has the effect of reducing excess
solder in all four corners of the pads. Sometimes in addition the overall
size is reduced by 1 or 2 mil.
An additional advantage is that the OVAL is a Gerber shape improving data
compactness, data sharing and interpretation reliability and it means that
for a single component there are no 'left' and 'right' or 'top' and 'bottom'
apertures (or D-codes).
Have fun,
Ahne.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of peter lee
Sent: Friday, April 26, 2002 07:58
To: [log in to unmask]
Subject: [TN] 0402 stencil apperture design
Has anyone used a "D"-shape 0402 land pattern on their
design?
The pad dimensions are 18x19mils (semi-circle on the
other ends) and 16mil spacing between the 2 pads.
What would be the stencil apperture recommendation for
the above design? We've used round pads for 0402s and
15% apperture reduction before.
Rgds,
Peter
__________________________________________________
Do You Yahoo!?
Yahoo! Games - play chess, backgammon, pool and more
http://games.yahoo.com/
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|