Excellent pictures Steve!!! In my previous life we used Metro circuirts
and there Conductive Epoxy fill and that seemed to work real well. Before
that we had all kinds of problems making people believe that via's in pads
are bad/ You know that those RF guys like to have every circuit grounded
as many times and often as they can. Like you said they fill up the pads
with via's and when you tell them it will not work they say "come on you,
you can't be serious". And when you spend all that time reworking those
spots because Quality saids "Insufficient solder" the engineer says "You
must not have printed your paste right" And it is then that you pick up
that Ball peen Hammer and chase him around the building.
[log in to unmask]
COM To: [log in to unmask]
Sent by: cc:
TechNet Subject: Re: [TN] Vias in pads
<[log in to unmask]
RG>
04/03/02 04:45
PM
Please respond
to "TechNet
E-Mail
Forum.";
Please respond
to SteveZeva
Ahhh vias in pads...what timing. In fact built a board last week that I had
no idea
that they put vias in the pads until the bare fab showed up. Soon as I seen
it I was
screaming like a banshee!!
Them: What's wrong Steve? Why are you so wound-up?
Me: Because there's vias in the pads!!
Them: Is that really a problem? Won't the solder just fill them up?
Me: Yes it will...and take all the solder away from the fillet to do it...
Them: Oh it can't be that bad, the via is so small...
Me: Okay, trust me on this...you'll see.
Go to: http://www.stevezeva.homestead.com and tell me I was right.
Luckily, this is just a pre-production build of 10 boards...I think there
is going to be a redesign after this...hehehe
-Steve Gregory-
This problem is never ending. I'm working now on the ugliest R/F board
imagineable. It too has all your problems. However, I have a forward
thinking engineer who understands the issues involved as you state them.
We
are redesigning and he's recalculating to eliminate those issues. So, it
can
be done. No, unless you redesign, you have a lost cause notwighstanding
rework adn subsequentg chip cracking due to thermal issues related trying
to
solder the little mutha's.
You can add vias in pads only as micro types or those having been plugged
and plated over. Still a redesign exists.
On the same note, can someone recommend a good R/F and other electrical
performance tool that is relatively easy to use? Hell of a question I
know,
but consider the source.
MoonMan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|