TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Ken Carlile <[log in to unmask]>
Date:
Tue, 23 Apr 2002 23:11:38 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ken Carlile <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
We recently received a prototype batch of 4 boards and experienced 4 for 4
failing test.  Our techs sprayed down certain chips with Freeze Spray and
the board began working properly, at least for a short period of time.  I
have checked prior tech net postings and have found fantastic responses as
to why Freeze Spray can damage a the IC or board, but can anyone explain why
they would begin functioning properly.  Being a rookie component engineer I
can fully understand the issues related to freeze spray, but out techs and
design engineers are just going to point the finger since their units work
when sprayed.  To further complicate the matter the chips that are being
sprayed are not all the same manufacturer and I can easily rule out a
component failure.  Our senior engineer thinks that it may be timing related
since the main circuit being froze is the Altera PLD (20K400E) and related
circuitry.

Can anyone defend the use of Freeze Spray?

Can anyone present a logical failure mechanism?

/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\

The best Freeze Spray argument to date was Werner Engelmaier's:
http://jefry.ipc.org/scripts/wa.exe?A2=ind9907&L=TechNet&D=0&m=23823&P=55370

However this points to failure after spray not the opposite.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2