TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Bev Christian <[log in to unmask]>
Date:
Tue, 23 Apr 2002 07:54:48 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (77 lines)
Steve,
1) Do the vias go all the way through the board?
2) Are they connected to a massive ground plane?
3) Any way to test the parts BEFORE wave soldering?
4) I wonder if the parts are experiencing a latent dewetting

regards,
Bev Christian
Research in Motion

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: April 22, 2002 9:07 PM
To: [log in to unmask]
Subject: [TN] Secondary reflow over wave...


Hi All!

Got a situation here that I think is secondary reflow...

Have a board here that has some J-leaded DRAM that in functional test, they
can get the board to pass test by putting some pressure on top of some of
the
40-pin J-leaded DRAM's that are causing them to fail...

Out of SMT things look fine, but I have observed some boards that have
failed, show an unusual solder joint appearance after wave. The board is
"swiss-cheesed" with vias, and none of them are tented. Every pad has a via,
they alternate, some have .050" traces to the pad, some have .020" traces to
the pad.

Where we're seeing problems is where there is a bank of them (like a grid of
2 by 8 of them layed-out side by side).

I'm thinking secondary reflow because of the open vias...or could be CTE
mis-match between the part and the board. It's a .062" FR4 board, with
fairly
large 40-pin SOJ's, could be experiencing some hellacious mismatch, no? The
gull-wing parts we don't see the problem, even though the via placement is
the same standard as with the J-leaded parts...J-leads aren't as compliant?

Gonna hook-up the mole tomorrow, attaching it to one of the J-leaded parts
to
learn what it is seeing...will tell me a lot...

Just wondering if anybody else has run into this before...

-Steve Gregory-

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2