TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Earl Moon <[log in to unmask]>
Date:
Sat, 20 Apr 2002 07:04:23 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Glynn Shaw <[log in to unmask]>
Subject:
From:
Glynn Shaw <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"; format=flowed
Parts/Attachments:
text/plain (80 lines)
After reading this Earl, I figured I better go explain to the frontline
that if a customer asks for photomicrographs then they are asking for
pictures of their cross sections. So she asks: Do I need to dress up?
Should I hold them in my hand and smile? or Should I display them like
those actors holding coke cans in the movies?

PS: do you want jpg's or gif's?



At 06:06 AM 4/19/02 -0500, you wrote:
>George,
>
>Thank you very much for shedding some light on an important, to us all,
>subject. Sure glad, for us all, you stick around though you're obviously
>thought of as much more than a board person.
>
>As for my experiences, and some of my friends in the business, I used to get
>mostly "up front" consulting jobs. Now, I get mostly "fix it" type work. I'm
>not complaining but, as you said, there seems a new way of designing,
>fabricating, and assembling product.
>
>The two examples, of my supplier base that's been with me for years, are
>good examples of concurrent engineering staffs. Sanmina Hadco, in its
>Haverhill tech center, still has this capability and I desparately hope it
>continues but, with the closure of its assembly tech center in Austin, I
>have to wonder if the pendulum is swinging back to "traditional" sales
>techniques (used car type approach).
>
>Though still providing good product, some of the other PCB technical
>"giants" don't talk technical anymore. They and many assembly houses talk
>the talk of sales folks mostly telling us/me what we/I want to hear. What
>they don't understand is I want to hear technical content with their ability
>to back it up.
>
>As much as I love my favorite board shop, PE, I have had few in depth
>technical discussions with them. As one example, I requested
>photomicrographs to accompany slugs before and after thermal stress to
>visually confirm their report. I was asked, when questioning why no pics
>were avaialable, as very nice sales lady, apparently, asked "what is
>photomicrographs?"
>
>I recognize my client's management, as many other companies, have limited
>knowledge concerning PCB's. That, in my opinion, is whay they should look
>for folks having up front approaches to preventing defect, through DFM/CE,
>at the design level.
>
>As you say, we need more good young engineers having the knowledge, talent,
>desire, and ability to do this ever more important job as the technical
>world gets more complex. I sure look back on a different world, but don't we
>all. Was it any better, I think so when it came to PCB's.
>
>Earl
>
>---------------------------------------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
>SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2