Brian:
There are several vinyl based temporary peelable masks that should work.
These products can be applied by printing using an imaged screen, similar
to(non-photoimageable)permanent soldermask application. They normally
require a post application bake to achieve the proper chemical resistant
properties and release characteristics.
It should stand up to your electroplated Ni and Au processes. In some cases
it is somewhat of a pain to remove depending on the size and configuration,
but worth a try.
Lackwerke Peters GmbH, MacDermid, Electra and Alpha Metals all used to carry
these types of products.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Brian L. Guidi [mailto:[log in to unmask]]
Sent: Friday, April 19, 2002 12:45 PM
To: [log in to unmask]
Subject: [TN] Peelable Soldermask
Good afternoon fellow techies...
I am searching for information on peelable soldermask, or an
acceptable alternative. I have an application which requires temporary
coverage of immersion gold plated fingers, through subsequent wet process
operations (additional 'electrolytic' gold plating). I need to cover the
fingers so they do not plate up when the electro-deposited gold is added
(the nets are connected) to the other end of the board. The situation is
complicated by the fact that the area requiring coverage is approximately
.012" below the external surface of the board, therefore standard
etch/plate dryfilm is not practical due to voiding. I'll try to provide a
mental picture: Imaging a rectangular board 2" long by .500" wide. It's a 6
layer board. On one end, a portion of L4/5 about .750" long, extends beyond
the rest of the part (along the length) about .400". These "wings" are the
portion requiring coverage during the plating process that is happening at
the other end of the board.
Platers tape has been ruled out as an option due to volume. The plan
is to apply a dryfilm soldermask to the external board surfaces to
permanently protect/insulate the via's, and then apply a peelable mask over
the same area which would conform to the 'drop-down' (.012") and cover the
exposed fingers on L4/5. The peelable soldermask would then be removed to
expose the fingers to the cleaning solutions.
I am looking for material recommendations, vendors providing peelable
mask application services, and any practical experience anyone has had with
a similar situation. I hope the explanation is not too foggy. It is Friday
after all, and I have a meeting with Sam Adams in about an hour and a half!
Thanks in advance for your help and insight...
Brian Guidi
Product Engineer
Teledyne Electronic Technologies
Tel: (603) 889-6191 X:310
Fax: (603) 886-2977
E-mail: [log in to unmask]
Any technical information attached to this document is intended for the
recipient only. Also, the export and use of the information is regulated
by the export laws of the United States. Diversion contrary to U.S. law is
prohibited. U.S. law prohibits sharing this information with any end-user
for any end-use related to the design, development, production, stockpiling
or use of chemical, biological or nuclear weapons or missiles, without the
prior approval of the United States Government.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|