Jana:
You have asked a BIG question.
There really is no known absolute answer.
Organics tend to discolor, if they have any sort of reactivity left in them,
and often, under the right circumstances even if they do not have any
reactivity left in them.
The general rule is they turn dark(er). The reactions are many, and clearly
going to be dependent on the base material. Discoloration is driven by heat,
and often exposure to sunlight.
Not to get too technical, but polymers (laminate, and soldermask, for
example) only rarely really react fully, and there is almost always some
unreacted polymer (called monomer when it is totally unreacted, and oligomer
when it is partially reacted) lurking in the matrix. When this contacts air,
water, and heat and UV, all sorts of unexpected things happen. In fact,
these very polymers often have added "preservatives" to prevent these
post-polymerization reactions from occurring.
The bottom line is (as if this really has ANY significanse in our industry)
that this discoloration rarely affects the physical properties of the
polymer. I think a great English playwright described this situation
centuries ago..."Much ado about nothing"?
Rudy Sedlak
RD Chemical Company
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|