In my opinion slight colouration differences between batches is not abnormal
but I do mean slight. I would need to know the material build to determine
if it could be a problem. Regards Steve Kelly
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Houston, Terri
Sent: Thursday, April 11, 2002 8:55 AM
To: [log in to unmask]
Subject: [TN] Coloration differences between batches of flex circuits
Hi folks,
We recently received a batch of 3-layer flex circuits, which were much
darker in color from the previous batch received (think copper colored vs.
chocolate colored).
I was told that the darker batch received a longer bake and that the
coloration difference was cosmetic.
Since I don't have a lot of experience with flex, I'm looking for input from
flex manufacturers/users on whether color differences between batches are
common and acceptable.
Thanks in advance,
Terri
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|