Rodney-
That's kinda my point.
base 2oz.=.0028... plating=.001... so base of 2oz. + min avg. plating
=.0038, or 0.0965MM.
But IPC spec says min thickness for 2oz base AFTER plating=76uM (0.076mm).
But thanks for the response...
-Chris
========
Chris,
Check your conversion numbers, 2oz copper should be .0028" or .003" rounded
up.
Rodney
"This e-mail message is intended only for the use of the named
recipient(s).
The information contained therein may be confidential or privileged, and
its
disclosure or reproduction is strictly prohibited. If you are not the named
recipient, please return it immediately to its sender at the above address
and destroy it."
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|