In anticipation of this, our drawings call for laminate or prepreg to be
FR-4.  Some boards we leave it to the discretion of the fabricator as far as
construction.  You could add "per IPC-4101" and copper foil per the
appropriate IPC doc just to make sure.
Not surprising, since many multilayer boards are done w/foil lam to reduce
$$$.  Just be sure to use a general specification to cover yourself and
communicate to your supplier what you want to end product to be made of or
spec'ed to.

Roger M. Stoops,  CID   [log in to unmask]


 -----Original Message-----
From:   [log in to unmask] [mailto:[log in to unmask]]
Sent:   Monday, March 18, 2002 11:05 AM
To:     [log in to unmask]
Subject:        [TN] Foil Lamination

The call-out on our fab drawings states to use copper clad epoxy laminate
FR4 base material. Our supplier in the past has purchased and certified
material to IPC-4101. We have now found out they have incorporated foil
lamination into their process. What type of requirements should we impose or
verify?
Thanks for your help!
Rick Howieson

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives