We thought of that and it seems one very logical thing to do. The only
problem is that
the boards are coated at our supplier's plant. And you know how QA persons
are...
how can we prove that the aluminum part was coated at the same time then the
batch
etc...
We have to monitor our supplier and got solid evidences.
Thank you all! If any other idea has not been through yet don't hesitate...
I'm all ears...
or all EYES!
JF
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Thursday, March 14, 2002 12:48 PM
To: [log in to unmask]
Subject: Re: [TN] Coating thickness
I agree with Brian. We place a 2x3" piece of aluminum plate next to the
assembly during coating, which gets coated at the same time. A part of the
plate is masked with tape so you can measure before and after cure.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Brian Ellis [SMTP:[log in to unmask]]
Sent: Thursday, March 14, 2002 10:46 AM
To: [log in to unmask]
Subject: Re: [TN] Coating thickness
Jean-François
Coat a lump of metal at the same time and use that to measure the
thickness.
Brian
"Bissonnette, Jean-Francois" wrote:
>
> Hi All,
>
> Does anyone now of a technique or system to check conformal
coating
> thickness after it's dry on production units? We have a
positector to
> measure paint thickness on our enclosures but they're not design
to
> work on materials like PCB.
>
> Jean-François Bissonnette
> Vérificateur, Contrôle de la Qualité
> Électronique
> Produits et Procédés
> Vapor Rail Inc.
> 10655 Henri-Bourassa O.
> St-Laurent, Qc
> H4S 1A1
>
> (514) 335-4200 x2021
> (514) 335-4231 fax
>
> <<Bissonnette, Jean-Francois.vcf>>
>
> WABTEC CORPORATION CONFIDENTIALITY NOTE
> The content contained in this e-mail transmission is legally
privileged and confidential information intended only for the use of the
individual or entity named herein. If the reader of this transmission is not
the intended recipient, you are hereby notified that any dissemination,
distribution, or copying of this transmission is strictly prohibited.
>
>
----------------------------------------------------------------------------
-----
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
>
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|