Hi MoonMan, Peter, et al,
In a message dated 03/07/2002 0:38:57, [log in to unmask]  writes:
>Actually, instead of more discussion on my part, IPC 2221, etc., and 6012
>cover all the ground, and much more, you are concerned about. There's
>little else to say.
Well, that is not quite accurate, neither document adequately addresses the
reliabiliity issues--for that  you need to go to IPC-D-279.
IPC-D-279 also will help you correlate some of the info; additional helpcan
be found in IPC-TR-486 and IPC-TR-579.
Any copper barrel plating thickness below 1.0 mils should be considered
especially vulnerable.

Werner Engelmaier

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2