Hi Jim,
the actual test method is in IPC-TM-650 (2.4.22). This one is not very
specific in defining what actually should be measured (panel or single
board). Still, para 3 says "The test specimens shall be in the form of
either printed boards or multiple printed panels". Then the drawing and the
procedure show a rectangular element that is measured, in my opinion this
shall be the panel.
If the above mentioned rectangular element is not to be the panel, ask the
board fab to singulate each individual board, measure it for warp, just to
make sure it checks out OK and then re-assemble them in panels. But, like
somebody was saying yesterday, talking about PGAs, this could be ignored.
Regards,
Ioan
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Thursday, March 14, 2002 8:21 AM
> To: [log in to unmask]
> Subject: Re: [TN] Board Bow and Twist two answers
>
> Hi Jim
> This is not a question where "the most votes" determines the answer.
> The last sentence in para 3.4.4 states Panels which contain multiple
> printed
> boards which are assembled on the panel and later separated SHALL be
> assessed
> in panel form.
>
> Susan Mansilla
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|