Hi Nancy,
Youngs Modulus is another name for Modulus of Elasticity [E], named so after
the first discoverer of the elastic behavior graphed in a stress-strain
diagram.
For non-creeping metals E is a unique constant; however, because the
creep-behavior of solder at the Ts we are using it it does not have a unique
stress-strain diagram or a constant E--they are T- and strain-rate-dependent
and you therefore have an infinite number of such diagrams/Es.
A crosshead is the moving [upper] clamp of a tensile test machine and its
rate of travel applying strain to the test specimen is referred to as
crosshead speed--it determines the strain rate.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|