From: | [log in to unmask][log in to unmask], 6 Mar 2002 07:45:55 -0500581_iso-8859-1 Phil, call me old fashioned, but I prefer Weller as a first choice and Metcal as a last choice. I have always had good results with Weller. Weller has a variety of types and styles to chose from and the ones I used were pretty much low maintenance. Ron Dieselberg Trainer/Auditor CMC ELECTRONICS CINCINNATI [log in to unmask]-----Original Message----- From: Phil Nutting [mailto:[log in to unmask]] Sent: Tuesday, March 05, 2002 14:45 PM To: [log in to unmask]Subject: [TN] I need a better soldering iron [...]45_6Mar200207:45: [log in to unmask] |
Reply To: | TechNet E-Mail Forum. |
Date: | Tue, 19 Mar 2002 10:47:36 EST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Grant,
Without actually seeing the boards I cannot be 100 percent.... but
Passing this around the table it is thought it could be incomplete mask cure
from incomplete volatile excursion or incomplete cross polymerization. These
can be cleared up with a double pass through a UV tunnel at correct intensity
and belt speed. Relative to conformal coating, I have assembled and coated
parts of this description without any problems; adhesion, outgas, or
otherwise. This would be the nice scenario.
A worse case condition is the boards were not completely dried after cleaning
prior to soldermask. The result being entrapments being forced out the vias.
The final bake (or boiling in this case) is especially hard on tented,
plugged or flooded vias will exhibit the "hues" or halo's, worsening to
actual blistering. In this condition it is the call of the board shop QA
prior to shipping.
One "cure" test is cotton swab with iso-al; green denotes cure issue.
The adhesion test: 3/4" wide tape pull at 90 deg with force.
One last thing, with the decreasing thickness of solder mask there can be an
absence or decrease of actual pigment on top of lands (traces, vias, etc).
If your discoloration includes flat areas this is probably not the case.
Boston Brad
781 858 0783
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|