Carl,
This ought to stir the pot!
In my thirty plus years in this business I've seen arguments both ways.
In my current life we will solder after crimping lugs which carry high current.
An argument could also be made for using a moisture barrier like "No-alox" as used in electrical wiring with aluminum conductors.
My late father-in-law used Vaseline on all the electrical connections for his comm-nav gear on his motorboat to prevent the salt from corroding the connections.
The point here is there may be a good reason for any of the combinations listed here or by my peers.
Just one man's opinion.
Phil Nutting
-----Original Message-----
From: Carl VanWormer [mailto:[log in to unmask]]
Sent: Wednesday, March 13, 2002 2:35 PM
To: [log in to unmask]
Subject: [TN] Soldering crimp connectors
We have a customer who insists that we solder our crimp connectors (after
crimping). He has had corrosion problems and is convinced that this is the
best solution. Is this a good thing? Are there any downsides we should
point out to help educate him?
Carl Van Wormer
Cipher Systems
1815 NW 169th Place, Suite 5010
Beaverton, OR 97006
Phone (503)-617-7447 Fax (503)-617-6550
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|