Well any time you introduce additional metals to a connection you are
actually increasing your risk of galvanic corrosion. Depending on the
design of the connector in question there are probably some purely
mechanical concerns as well. The connector manufacturer will almost
certainly have recommended uses. They would probably be your best bet. It
might end up just being a mechanical tolerance or malleability issue.
Good Luck
-----Original Message-----
From: Carl VanWormer [mailto:[log in to unmask]]
Sent: Wednesday, March 13, 2002 12:35 PM
To: [log in to unmask]
Subject: [TN] Soldering crimp connectors
We have a customer who insists that we solder our crimp connectors (after
crimping). He has had corrosion problems and is convinced that this is the
best solution. Is this a good thing? Are there any downsides we should
point out to help educate him?
Carl Van Wormer
Cipher Systems
1815 NW 169th Place, Suite 5010
Beaverton, OR 97006
Phone (503)-617-7447 Fax (503)-617-6550
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|