Sal ammoniac or ammonium chloride is the active component of one of the
most active soft-soldering fluxes ever. It has no place in electronics
assembly workshops. Its use could cause horrific ionic contamination and
consequent dendrite formation, corrosion and you-name-it. Furthermore,
its fumes are highly irritating and toxic. Forget it!
Brian
> "Dan R. Johnson" wrote:
>
> Why aren't sal amoniac blocks available from electronics suppliers any
> more? I found them from a stained glass supply house but am wondering
> why Kester et all stopped selling them. Any ideas out there?
> Dan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------