Jean-Francois
As St. Doug will likely say, "depends". Depends on how much ionic contamination, what voltage potential is present, and what you are doing with the board. It's my understanding that a coating may slow dendrite growth, all other factors being equil, but the only way to prevent dendrites is to avoid at least one of the holy trinity of dendrite growth (contamination, voltage, moisture).
The best protection - a clean board. If the end use environment is what is contaminating the boards, then yes - a coating would be a good protection. But as a bandaid solution, not good.
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
>>> [log in to unmask] 03/21/02 11:19AM >>>
Is conformal coating a good protection against dendrites? I read that
ionic contamination can cause dendrites, if a board has ionic contamination,
will conformal coating prevent dendrites?
Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1
(514) 335-4200 x2021
(514) 335-4231 fax
<<Bissonnette, Jean-Francois.vcf>>
WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|