What if the panels are bowed beyond the .75% limit, the boards are not, I
can build them and I can use them? I know I'm answering my own question, I
should use them, right? Well, what's the purpose of the .75% requirement?
I would think that the requirement should be whatever is agreed upon between
customer and supplier. If I can live with 2%, why not (within reason).
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Franklin D Asbell [SMTP:[log in to unmask]]
Sent: Thursday, March 14, 2002 8:25 AM
To: [log in to unmask]
Subject: Re: [TN] Board Bow and Twist
James,
An afterthought, the bow and twist requirement is there to provide
ease of
board population as well as end use fit. If the board is warped
prior to
assembly, this indeed would affect population thus potentially
making the
boards unsuitable for end use...just something to think about, or
pass along
to your supplier.
Franklin
----- Original Message -----
From: "Marsico, James" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 14, 2002 6:48 AM
Subject: [TN] Board Bow and Twist
> I think this is a no-brainer, but here goes... We were delivered
boards
in
> panel form from one of our suppliers. At Incoming Inspection, the
panel
was
> rejected for excessive bow (>75% for SMT) and returned the
supplier. The
> supplier called me and said that even though the panel exceeded
the bow
> requirement, the individual boards were acceptable. When I quoted
the bow
> and twist requirement from IPC-6012, "Panels which contain
multiple
printed
> boards which are assembled on the panel and later separated shall
be
> assessed in panel form." , he said yes, you measure the individual
boards
in
> the panel. I need clarification.
> Thanks,
> Jim Marsico
> Senior Engineer
> Production Engineering
> EDO Electronics Systems Group
> [log in to unmask] <mailto:[log in to unmask]>
> 631-595-5879
>
>
--------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following
text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
[log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315
>
--------------------------------------------------------------------------
-------
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|