Thanks Steve,
I usually keep some good sections and other images too. Don't have anything
showing them with me on this computer. I'll find some and a surface shot of
the type of surface being discussed, another time.
I just can't get over what a really bad hole is shown but how really good
the surface plating is. Luck and no skill at work here. Funny thing is, I
didn't even know this board had been produced this way. Had an open
somewhere and buzzed it out and found a suspect are and sectioned it. Wala,
a blind, plated over via with no plating in the hole. I can't believe the
shop, who did very little in terms of sophistication, actually did the
sequential lamination and plated over the resin so well.
Earl
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|