Jorge
To my knowledge there is nothing that will do this job long-term.
You can try Paralene - Silicone - Acrylics - Urethanes etc., but underwater?
Not in my experience.
Occasional flood? What about the connector and other uncoated items? And
what quality the rain water - acid rain?
Better to have a drain hole in the box to let it out, then you can probably
successfully use any of the above as you prefer - but keeping in mind the
pro's and con's of each.
Regards Graham Naisbitt
[log in to unmask] <mailto:[log in to unmask]>
Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK
www.concoat.co.uk <http://www.concoat.co.uk>
Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Jorge Santana
> Sent: 29 March 2002 17:06
> To: [log in to unmask]
> Subject: [TN] Underwater application
>
>
> Hi
>
> We need found out a way to keep the board working in a underwater
> environment, there is possibilities of occasional flood inside the box
> enclosure and the board has to survive, the water came from rain.
> Folks from automotive world " under hood applications" have this
> experience since cars are subject to flood also.
>
> What kind of material is used ? What recommended thickness ?
>
> We are thinking about RTV Elastomeric Conformal Coating.
> It is not necessary to say that the solution should be not
> expensive and
> effective.
>
> Thanks
> Jorge Santana
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|