Hi Technetters,
Can anyone help me?
We are curently running some BGA'S through reflow, and on inspecting them
through our Ersascope BGA inspection system have measured there is a ball
drop of around 30% from original ball size. The actual ball formation looks
very "border line" as in, has it single or double dropped. Does anyone know
the guidlines for such a drop? Is 30% the bottom end tolerance and if so
should I be looking at a drop of + 30% to insure a good looking sound joint
on the BGA.
Many thanks in advance,
Adrian Hanks.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|