Mr. Furrow,
So, you are saying that I should go below 10 mil finished hole size then what is
your recommended finish hole size. I definitely need to change from 10 mil +3 /
-10 to 10 mil +0 / -10. And yes my board is 62 mil thick.
re,
ken patel
"Furrow, Robert Gordon (Bob)" wrote:
> Ken,
>
> No wonder you are having problems, your finished hole size is way too big
> for your pad, and the volume of paste able to be deposited onto the pad. I
> would typically require a finished hole size of 10 mil + 0 / - 10. With 0603
> pad sizes even this is not sufficient and you need to go even smaller with
> the finished hole size. I am assuming you are talking an 0.063 inch board
> thickness.
>
> Thanks,
> Robert Furrow
> Printed Wiring Board Engineer
> Supply Chain Networks
> Lucent Technologies
> 978-960-3224 [log in to unmask]
>
> -----Original Message-----
> From: Ken Patel [mailto:[log in to unmask]]
> Sent: Tuesday, March 05, 2002 2:11 PM
> To: [log in to unmask]
> Subject: Re: [TN] Via in Pad? Need Help!!!
>
> We have via in pad of 603 and bigger size components including RF filters.
> The
> via size is 10 mil +3 /-10.
>
> re,
> ken patel
>
> Kathy Kuhlow wrote:
>
> > What type of component package?
> >
> > Kathy
> >
> > ------------------------------------------------------------------------
> >
> > TEXT.htmName: TEXT.htm
> > Type: Plain Text (text/plain)
>
> ----------------------------------------------------------------------------
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ----------------------------------------------------------------------------
> -----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|