TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
"Marsico, James" <[log in to unmask]>
Date:
Tue, 5 Mar 2002 09:58:02 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Parts/Attachments:
text/plain (181 lines)
Couldn't you temporarily mask the bottom of the vias with tape, then remove
the tape after reflow?  Wouldn't the void be open on the bottom side of the
board?  

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]> 
631-595-5879


        -----Original Message-----
        From:   Marki Sasportas [SMTP:[log in to unmask]]
        Sent:   Tuesday, March 05, 2002 7:00 AM
        To:     [log in to unmask]
        Subject:        Re: [TN] Via in Pad? Need Help!!!

        Hello Siggi,
        We had the same problem, 
        1) Using HASL finish to the board will not help you because as Brain
Ellis
        said the amount of solder that drains down the via is much more then
you
        supply (coat + print )- we tried it without success.
        2)  DO not Mask the Vias from the bottom side it will cause very big
voids.
        3)  You can try to seal the vias with paste but note that if it will
have
        height it can cause problem during printing.
        4) I recommend you to use blind microvias or just take the holes out
of the
        pads.

        Regards,
        Marki Sasportas. 

        -----Original Message-----
        From: Zweigart, Siegmund [mailto:[log in to unmask]]
        Sent: Tuesday, March 05, 2002 9:53 AM
        To: [log in to unmask]
        Subject: Re: [TN] Via in Pad? Need Help!!!

        Hello Ken

        We had the same problem (or still have).
        We tried HASL and OCC Boards but there was no difference.
        We also tried plugging with a special stencil and 63/37 but this
don't
        works.
        We did not try a high temperature solder.
        Masking is quite critical because of voids.
        Beside redesign you have only one chance: Look for new process
parameters.

        Siggi


                ----------
                From:  Ken Patel [SMTP:[log in to unmask]]
                Sent:  Montag, 4. März 2002 23:37
                To:  [log in to unmask]
                Subject:  [TN] Via in Pad? Need Help!!!
                Importance:  High

                Guys,
                On our nickel gold board, solder joints are below IPC spec
        (insufficient
                solder) where there are vias in pad. Solder is drained down
the via
                holes and deprived the joint of necessary solder.  I would
like to
        know
                the following.
                (1) How about using the surface finish 63/37 coating HASL
instead of
                Ni-Gold? I think gold dissolves in solder so quickly that I
rather
        use
                HASL processed boards, any thoughts?
                (2) Do you guys mask the via on bottom side to avoid solder
draining
        out
                on the other side?
                (3) Does anybody try Hi Temp solder paste to fill the vias
as our
                assembly house ordered via stencils to fill the via using
eutectic
                (63/37) solder paste which didn't work?

                Looking for
                re,
                Ken Patel

               
	
----------------------------------------------------------------------------
        -----
                Technet Mail List provided as a free service by IPC using
LISTSERV
        1.8d
                To unsubscribe, send a message to [log in to unmask] with
following
        text in
                the BODY (NOT the subject field): SIGNOFF Technet
                To temporarily halt delivery of Technet send e-mail to
        [log in to unmask]: SET Technet NOMAIL
                To receive ONE mailing per day of all the posts: send e-mail
to
        [log in to unmask]: SET Technet Digest
                Search previous postings at: www.ipc.org > On-Line Resources
&
        Databases > E-mail Archives
                Please visit IPC web site http://www.ipc.org/html/forum.htm
for
        additional
                information, or contact Keach Sasamori at [log in to unmask] or
        847-509-9700 ext.5315
               
	
----------------------------------------------------------------------------
        -----

	
----------------------------------------------------------------------------
        -----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET
        Technet NOMAIL
        To receive ONE mailing per day of all the posts: send e-mail to
        [log in to unmask]: SET Technet Digest
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
        E-mail Archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
        ext.5315
	
----------------------------------------------------------------------------
        -----

	
----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
	
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2