Hi Franklin! Do you have any photos which Steve could post on his website?
Photos would be very helpful.
Dave Hillman
Rockwell Collins
[log in to unmask]
Franklin D Asbell <[log in to unmask]>@ipc.org> on 03/14/2002
07:23:11 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Franklin D Asbell <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Unusual plated 'stuff' on copper surface
This past January we began seeing unusual 'growths' ((for lack of better
descriptive wording)) on the surface of panels after copper II, they are
typically observed on one end of the panels, often only a couple panels
per tankload exhibit this.
These 'growths' look like fine strands of metal of fabric fibers, they are
clustered together like someone poor shavings there, and plated over them.
If any of you recall pics of those bacteria found in that Mars asteroid
from the Antarctic, they appear similar to that (not saying we have
bacteria growing in our baths of course). Occasionally we see this out
towards the center of panels, I don't believe we have ever seen all panels
in a tankload exhibit this either. This condition is observed on one or
two loads per day (out of about 20 - 30), some days not at all.
We started seeing this in one bath (of three in house) until recently it
appeared in another bath simultaneously.
Any help on this would be greatly appreciated as our process engineers,
lab techs, and suppliers are baffled.
Thanks,
Franklin D Asbell
Network Circuits, Inc.
Irving, Texas 75061
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|